Name of
Components |
Common Use |
Calorized Materials |
Memo |
| Class |
Life |
Class |
Life |
| 1 |
Snout
|
Stainless Casting
(DCS-9) |
10 months |
Calorized
Stainless
Casting(DCS-9) |
24 months |
Regularly supplying
(from 1992)
|
| 2 |
Snout
|
Stainless Casting
(CN12B) |
12 months |
Calorized
SUS316L
(Welded
Structure) |
under trial use
(from Dec., '98) |
|
| 3 |
Ingot Folk |
SUS316L
|
10 months |
Calorized
SUS316L |
30 months |
Regularly supplying |
| 4 |
Suction Pipe |
SUS316L
|
2-3 months |
Calorized
SUS316L |
6 months |
Regularly supplying |
| 5 |
Suction Pump Shaft |
SUS316L
|
2 months |
Calorized
SUS316L |
4 months |
Regularly supplying |
| 6 |
Separator
|
SUS316L
|
6 months |
Calorized
SUS316L |
28 months |
Regularly supplying |
| 7 |
Bearing of Sink Roll |
SUS316L+
Thermal Spray |
15 days |
Calorized
SUS316L |
Trial scheduled |
|
| 8 |
Melting Pot |
SUS316L |
2 months |
Calorized
SUS316L |
Trial scheduled |
|
| 9 |
Sink Roll
|
SUS316L+
Thermal Spray |
6 months
|
Calorized
SUS316L |
Trial scheduled |
|
| 10 |
Straightening Vanes
of Sink Roll |
SUS316L |
1-2 months |
Calorized
SUS316L |
Trial scheduled |
|